Model Features
1、Heat affected zone is small, no deformation for precision molds.
2、Welding depth is large, welding firm. Sufficient fusion, no repair traces. No dimple phenomena at combining position of projection parts and bulge part of molten pool soluble material.
3、Low oxidation rate, the color of the processing parts is intact.
4、No stomata or sand hole disappeared after welding.
5、The welding parts can be processed, especially suitable for polishing requirements of the mould repair.
6、The processing parts can reach to 50 to 60 rockwell hardness.
Applications display
Repairing and welding for crack, corner breakage, touched edge and damaged sealing side of mould, precision injection molding, die-casting, stamping, stainless steel and other horniness.
High accuracy, laser spot diameter is only 0.2mm ~ 1.5mm. Little heat effect area, no deformation of the processing parts;no effect for etch after welding.